(Institución)
 
 

Docu-menta > Laboratorio Nacional de Fusión > Artículos del Laboratorio Nacional de Fusión >

Por favor, use este identificador para citar o enlazar este ítem: http://documenta.ciemat.es/handle/123456789/3888

Título : Study of deuterium permeation, retention, and desorption in SiC coatings submitted to relevant conditions for breeder blanket applications: thermal cycling effect under electron irradiation and oxygen exposure
Autor : Hernández Díaz, Teresa
Palabras clave : SiC coating
tritium permeation
Fecha de publicación : 2021
Editorial : Journal of Nuclear Materials
Citación : Journal of Nuclear Materials 557 (2021) 153219
Resumen : In this paper we report on the performance as deuterium permeation barriers of sputtered amorphous, dense and not fully stoichiometric SiC coatings under relevant conditions for breeder blanket applications in fusion reactors. To do that, we investigate the following effects on permeation values: (i) thermal cy- cling at 450 °C, (ii) combined thermal cycling and e −irradiation (1.8 MeV up to a total dose of 1 MGy), as well as (iii) oxygen exposure at a temperature of 450 °C during e −irradiation. Data show that the permeation reduction factor (PRF) for the as-deposited SiC coated is ∼10 4 , even at the predicted opera- tion temperature for the breeder and it is slightly reduced either by thermal cycling without and during e −irradiation. However, the exposure to oxygen at 450 °C during e −irradiation leads to degradation of the coating and of its PRF of about three orders of magnitude. The origin of the coating degradation is discussed. We also study the D retention and desorption in SiC coatings that were implanted with D at energy of 7.5 keV prior to (as-deposited) and after being submitted to the treatments previously described. Sec- ondary ion mass spectroscopy data show that thermal cycling, without and during e −irradiation, strongly increases the D retention in the coatings and leads to the appearance of D 2 desorption peak at temper- atures between ∼400-750 °C, whereas e-irradiation during thermal cycling does not significantly change the D retention but shifts to higher temperatures thisD 2 desorption peak
URI : http://documenta.ciemat.es/handle/123456789/3888
Aparece en las colecciones: Artículos del Laboratorio Nacional de Fusión

Ficheros en este ítem:

Fichero Descripción Tamaño Formato
Hernandez D perm SiC coating thermal cycling 2021.pdf3.05 MBAdobe PDFVisualizar/Abrir
View Statistics

Los ítems de Docu-menta están protegidos por una Licencia Creative Commons, con derechos reservados.

 

Información y consultas: documenta@ciemat.es | Documento legal